Edge Rewrite
// HTMLRewriter · presentation

This page was redesigned at the edge.

Cloudflare fetched the original article and streamed it through HTMLRewriter to apply an entirely new visual system without rebuilding the source page.

// request.cf · coarse context

A page that knows where it met you.

Only coarse request metadata is shown. This demo does not display or persist visitor IP addresses.

Country
US
Cloudflare location
CMH
Connection
HTTP/2
Language
Not provided

Ray ID: a2249107ea9e18aa

Jump to content

Talk:Resin casting

Page contents not supported in other languages.
Add topic
From Wikipedia, the free encyclopedia
Latest comment: 12 years ago by Bizzybody in topic Details and mold life.

Details and mold life.

[edit]

There are some platinum cure RTV silicones that can be used for molds that will withstand 1,000 or more castings with little or no loss of detail, when used with the right mold release compounds and compatible resins. From a glossy surface original, RTV silicone can reproduce details as fine as fingerprints, and replicate them in the castings. Soft urethane rubber can be used to make molds at less cost than silicone, but extreme care must be taken with applying mold release when casting urethane resin in urethane rubber molds because the resin will easily and permanently bond to the rubber. There are two main types of RTV silicone used for making molds. Platinum cure, which is the most expensive but has a very long shelf life for cured molds and can be formulated to have essentially zero shrinkage. Platinum cure is also compatible with the widest variety of resins. Tin cure is slightly less expensive but the molds will eventually deteriorate even when not used, and it also inhibits the cure of some types of resins and platinum cure silicone. Tin cure silicone exhibits more shrinkage than platinum cure. Bizzybody (talk) 05:08, 2 June 2014 (UTC)Reply